Skip to content
China Steel Supply

Cold Rolled Steel Grades Equivalent Chart

Cross-reference chart: EN 10130 DC01-DC06, JIS SPCC-SPCF, DIN St12-St14, ASTM A1008 CS/DS/DDS/EDDS, GOST 08ps/08Yu, IS 513 CR1-CR5. Pick the right cold rolled grade and get a 24h quote.

Factory-direct export support Mill certificates and packing guidance Response by email, phone and WhatsApp

Cold rolled steel grades are named differently in every market: a European drawing says DC04, a Japanese die shop says SPCE, an American order says DDS, a Russian contract says 08ю, an Indian tender says CR3. This chart cross-references the five common quality levels across EN 10130, DIN 1623, JIS G3141, ASTM A1008, GOST 9045, IS 513 and GB/T 5213 so buyers and engineers can specify the right coil the first time.

Quote Any Cold Rolled Grade — DC01-DC06, SPCC-SPCF, CS-EDDS, 08пс/08ю, CR1-CR5

Send thickness, width, temper, surface finish, quantity and destination port. ChinaCNU Steel will reply with a workable factory quotation within 24 hours.

  • MOQ from 25 tons, sample and trial order discussion available.
  • Mill test certificate (chemistry + mechanical properties) with every coil.
  • Payment by T/T or L/C according to order size and buyer profile.

Request 24h Quote WhatsApp Sales

Cold Rolled Steel Grade Equivalent Chart

Quality level EN 10130
(Europe)
DIN 1623
(old German)
JIS G3141
(Japan)
ASTM A1008
(USA)
GOST 9045
(Russia/CIS)
IS 513
(India)
GB/T 5213
(China)
Typical use
Commercial quality (CQ) DC01 St12 SPCC CS Type A/B 08пс CR1 DC01 Bending, tube, panels, galvanizing base
Drawing quality (DQ) DC03 St13 SPCD DS Type B 08пс ВГ CR2 DC03 Moderate draws, wheels, cases
Deep drawing (DDQ) DC04 St14 SPCE DDS 08ю (08Yu) CR3 / CR4 DC04 Sinks, housings, auto inner panels
Special deep drawing (SDDQ) DC05 St15 SPCE / SPCF DDS / EDDS 08ю ВОСВ CR4 DC05 Severe multi-stage draws, auto panels
Extra deep drawing, IF steel (EDDS) DC06 SPCF / SPCG EDDS 01юТ CR5 DC06 Most severe draws, exposed auto skins

Matches are commercial approximations. Chemistry limits and guaranteed r/n values differ slightly between standards — when a die trial or certification depends on it, specify mechanical minimums on the purchase order rather than relying on the grade name alone.

Mechanical Properties by DC Grade (EN 10130)

Grade Yield ReL (MPa) Tensile Rm (MPa) A80 (%) r90 n90
DC01 140–280 270–410 ≥ 28
DC03 140–240 270–370 ≥ 34 ≥ 1.3
DC04 140–210 270–350 ≥ 38 ≥ 1.6 ≥ 0.180
DC05 140–180 270–330 ≥ 40 ≥ 1.9 ≥ 0.203
DC06 120–170 270–330 ≥ 38 ≥ 2.1 ≥ 0.220

How to Choose the Right Grade

  • Bending, tube, panels, galvanizing base: DC01 / SPCC — lowest cost, widest availability.
  • Moderate draws: DC03 / SPCD — guaranteed r-value begins here.
  • Deep drawing: DC04 / SPCE / DDS — the standard DDQ choice.
  • Severe or multi-stage draws: DC05 — specify when DC04 fails the die trial.
  • Most extreme draws / exposed skins: DC06 (IF steel) — titanium-stabilised, highest formability.

Old DIN St12 / St13 / St14 Still on Your Drawings?

Many Middle East, African and Iranian buyers still order ST12, ST13 and ST14 from legacy German drawings. DIN 1623 was superseded by EN 10130: ST12 → DC01, ST13 → DC03, ST14 → DC04. We accept RFQs in either naming and confirm the EN grade on the mill test certificate.

FAQ

Is SPCC equal to DC01?

Commercially yes. Both are commercial-quality CRC; JIS allows slightly higher P/S. See the detailed SPCC vs DC01 comparison.

What is the ASTM equivalent of DC04?

DDS (Deep Drawing Steel) under ASTM A1008. For DC05-level performance, specify DDS with agreed r/n minimums or EDDS.

What is 08ю steel?

08ю (08Yu) is the aluminium-killed deep drawing grade under GOST 9045 used across Russia and the CIS — the working equivalent of DC04/DC05. We export it with EAC-market-friendly documentation.

Which grade for hot-dip galvanizing feed?

DC01/SPCC full hard is the common feed for continuous galvanizing lines with in-line annealing. See our hot rolled vs cold rolled for galvanizing guide.

Related Cold Rolled Steel Pages